I tried printing something on my bambu instead of my voron since I cant get the voron working properly. Why do the outer walls do this?
I tried printing something on my bambu instead of my voron since I cant get the voron working properly. Why do the outer walls do this?
8 Comments
oldfart@lemm.ee · 4 pts · 1y
Is the filament dry?
stealth_cookies@lemmy.ca · 3 pts · 1y
That the default petg profile? Bump up your temperature by 10C and try again. Their PETG profile is too cold for the flow rate.
muusemuuse@lemm.ee · 2 pts · 1y
I actually lowered it to 250 and turned off the fan and it didn’t help.
stealth_cookies@lemmy.ca · 3 pts · 1y
Wrong way to adjust, try printing at 265 and keep the part fan on ( aux fan off).
muusemuuse@lemm.ee · 2 pts · 1y
the spool says not to exceed 250
roofuskit@lemmy.world · 7 pts · 1y
Here's the thing about temperature sensors, they vary.
stealth_cookies@lemmy.ca · 3 pts · 1y
Run a temp tower if you are worried about it, but I run all PETG at 265 on my P1S. 255 will tear like you show and print matte which means it isn't properly melted.
SpikesOtherDog@ani.social · 2 pts · 1y
If I have to guess, it looks like compression. Either you are over extruding or your print head is too close.